Ferro-Titanit C-Spezial

The binder phase consists of a cold work steel containing 3% chromium and 3% molybdenum. The relatively low alloy content brings about a low tempering resistance. The hardness decreases above approximately 200 °C. In comparison with the other grades, C-Spezial has the best machining properties.

Download

Schematic "family tree"
Ferro-Titanit | PDF